BGA CHIPSET OBSERVE PRECAUTIONS FOR HANDLING
BGA Chips is MOISTURE SENSITIVE DEVICES. Devices require baking, before mounting, Here is the general bake-out process, Lay the BAG on the tray, and put it in to a baking dry cabinet. Set the temperature and time as: 125C x 24 hours or 80C x 48 hours
Pay attention to the difference between
leaded (Pb) balls and lead free (No Pb) balls.
Lead-free/No Pb BGA chips:
245C-260C(Maximun)
Leaded/Pb BGA chips:
180C-205C(Maximun)
Sufficient Stock
Na razie nie dodano żadnej recenzji.
16 other products in the same category
Samsung Exynos8895 templariusz
Samsung Exynos8895/MSM8998/S8+ templariusz
i32370M Stencil Template 90x90M (ang.)
I3-2370M SR0DR Stencil Template 90*90 (ang.)
Obsługa stacji BGA Solder Magnet90
ZQT-90X BGA Reballing Station 80*80 90*90 Stencils Reballing Station BGA Solder Station (ang.)
10in1 BGA96 BGA100 BGA132 BGA132 BGA152 BGA272 BGA316 2246XT 2258XT AS22585858BN
BGA96 BGA100 BGA132 BGA132 BGA152 BGA152 BGA272 BGA316 2246XT 2258XT AS225858585858XT AS225858585858